Low resilience can make compression loads smaller.
Close contact can make contact resistance smaller.
| Item | Unit | HN-012-T | |
| Thermal Conductivity | W/mK | 1.2 | |
| Thickness | mm | Standard | 1.0,1.5,2.0 |
| Order made | 3.0 | ||
| Hardness | ASKER-C | 20 - 22 | |
| Tensile Strength | MPa | 0.24 | |
| Elongation at Break | % | 106 | |
| Adhesive Strength | N/25mm | 2.20 | |
| Flammability | UL-94 | ≧0.3mm | V-2* |
| ≧1.0mm | V-0* | ||
| Dielectric Breakdown Voltage | kV/mm | 8.4 | |
| Volume Resistivity | Ω•cm | 1.5×1010 | |